I think that is a misleading generalisation. There is a lot of excellent information available from the Nickel Institute free of charge, as downloads. All you have to do is search the site for what you want and register - it is entirely free. You can then download vast quantities of good and reliable information about nickel, its alloys, how to weld it, etc. I'd suggest you visit www.nickelinstitute.org.
Regards,
Owen.
----- Original Message -----From: basem aliSent: Sunday, October 18, 2009 7:18 AMSubject: [MW:3516] Re: sour service
Because Nickel is highly susceptible to stress corrosion cracking even with the presence of a small amount of sulfide compound.
--- On Thu, 10/15/09, Ali Asghari <asghariali@rocketmail.com> wrote:
From: Ali Asghari <asghariali@rocketmail.com>
Subject: [MW:3506] sour service
To: materials-welding@googlegroups.com
Date: Thursday, October 15, 2009, 4:05 AM
hi allwhy Ni is detrimental effect for corrosion property in sour service?regards.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Comments