[MW:3511] RE: 3508] Re: Stainless Steel WPS

Hi,
With proper selection of coated electrode and qualified WPS / Qualified welder, you can weld SS (any grade) even to radiography quality. Coated electrodes are available in the market.
 
Regards,
 
R.Gopalasamy,
Sr.QA/QC Consultant,
Hindustan Oil Exploration Company Ltd,
PY1, Onshore Gas Processing Facility,
Thirukkadaiyur.
email : rgopalasamy @hoec.com
Mobile : 09789090752


-------------------------------------------------------------------- HOEC Email Disclaimer : http://www.hoec.com/email_disclaimer.htm



From: materials-welding@googlegroups.com on behalf of PREM SHANKARDUTT NAUTIYAL
Sent: Fri 10/16/2009 12:18 PM
To: mpatel@metalcare.com
Cc: materials-welding@googlegroups.com
Subject: [MW:3508] Re: Stainless Steel WPS


Hi

What type of joint are you talking about ?

If it is a single sided joint without access from other side, root + hot pass has to be welded by TIG. You cant use SMAW directly.

If there is access from other side and chip back is possible you can go for SMAW like double V full penetration joint..

Also you can weld partial penetration joint root with SMAW..

Regards

Prem Nautiyal

On Fri, 16 Oct 2009 11:50:08 +0530 wrote
>



Hi there,



One of our manager wants to Develop WPS for SS which can utilize
SMAW –root. I do not see it is common in SS welding. But there may be something
can make us competitive against GTAW root.



Does anybody have thought to share with me?



Thanks in Advance..!



Minal Patel










PREM S NAUTIYAL
CELL : 9820313278
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...