Minal Patel,
Lincoln Electric's STT process can be used as an alternative to open
root welding with stainless steel. It is a GMAW process that with
proper training and technique can yield high productivity.

Regards,
TF

On Oct 15, 11:29 pm, "Minal Patel \(Sorge's Welding\)"
<mpa...@metalcare.com> wrote:
> Hi there,
>
> One of our manager wants to Develop WPS for SS which can utilize SMAW -root.
> I do not see it is common in SS welding. But there may be something can make
> us competitive against GTAW root.
>
> Does anybody have thought to share with me?
>
> Thanks in Advance..!
>
> Minal Patel

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...