[MW:3474] Re: Grain size

Senthil,
It should be in the MTR. But a fine grain size starts from 6 up.
Shashank

--- On Sat, 10/10/09, MNS <mn.senthilkumar@ymail.com> wrote:

From: MNS <mn.senthilkumar@ymail.com>
Subject: [MW:3469] Grain size
To: "Materials & Welding" <materials-welding@googlegroups.com>
Date: Saturday, 10 October, 2009, 9:41 AM


May I know the Grain size of SA 516 Gr 70?


Thanks
Senthil


Now, send attachments up to 25MB with Yahoo! India Mail. Learn how
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...