Monday, April 28, 2008

[MW:755] Query on use of Body Material on test valve for Fire testing certification on Hastelloy Valve


Hi all,

I need your help for technical clarification for fire safe testing on Hastelloy Ball Valves.

We are buying soft seated Hastelloy On-Off ball valves, as per specifications all soft seated valves shall be fire safe design and a fire safe certificate is must.

The manufacturer is now taking up the Fire test at China but they are using the body material Austenitic SS (304 / 316). They claimed that the Hastelloy can be classified as 'Austenitic' within the generic classification defined in API 607.

I have a queries as below:
1.) Whether the Hastelloy material C-276 can be classified as Austenitic material within the generic classification defined in API 607. Please provide the reference that defines this.
2.) If the answer to 1.) is yes, whether testing on any austenitic material, say 304 or 316, can qualify the fire test capability of Hastelloy valves.

The relevant section of API 607 is appended below for your ready reference.





Thanks in advance,


Regards,

Sanjay Gandhi
DID : +65-65016099

Foster Wheeler Asia Pacific Private Limited
Block 7 #01-25
991 Alexandra Road
Singapore 119964
Tel: +65 6501 8888

======================================================= Confidentiality Notice  This communication and the information it contains:-  (a) Is intended for the person(s) or organisation(s) named above and for no other person(s) or organisation(s).   (b) May be confidential, legally privileged and protected in law. Unauthorised use, copying or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by email at Postmaster@fwuk.fwc.com. ======================================================= 
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...