Skip to main content

[MW:744] Re: 737] Re: how to find hydrogen concentration

Where from you take Rf?
Is H for Hydrogen % or partial pressure?
Finally how do you use Ph and  in what relation?
What are the reference books, standards in the above context.?
Regards,
tagore


On Wed, Apr 23, 2008 at 8:50 AM, Bathula Raghuram (Mumbai - PIPING) <R.Bathula@ticb.com> wrote:

the formula is not appering in the message, hence resending as an attachment.

-----Original Message-----
From: materials-welding@googlegroups.com on behalf of Raghuram Bathula
Sent: Wed 23/04/2008 20:51
To: materials-welding@googlegroups.com
Subject: [MW:737] Re: how to find hydrogen concentration

May i know why you need this calculation? if possible please detaile it for
the benifit of all members. probably the following would help you!

This formula is used for detecting cracking susceptibility of steels and is
valid only for certain range of steels



Where *P*H is the cracking susceptibility parameter, H is the concentration
of hydrogen (in parts per million), *R*f is the restraint stress (in
megapascals), and:




Good luck!

On Wed, Apr 23, 2008 at 3:28 PM, mech <arunmecheng@gmail.com> wrote:
>
> is there any mathematical formula to find  optimum level of hydrogen
> concentration in steels
>
> >
>









--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...