Skip to main content

[MW:750] HI I AM IN USA


Dear All,

 

Hi ,it is very glad to tell you all that our company has been authorised by AWS ( American society of welding) to conduct CWI certified welding and certiifcation programme.

 

I have been invited by AWS MIAMI HQ to take part in the international conferance here.

 

I am at present in NJ NEWJERSEY

 

HOTAL HOWARD JOHNSON EXPRESS IN

1025 RT 22 WEST NORTH PLAINFIELD  NJ 07060 PHONE 09087536500 

 

I will leave NJ on 27th morning.

 

I will remain in MIAMI -FLORIDA on 27th april night to Ist May morning .

 

My address at Miami is Hotel Airport Mariott Miami.

 

If any body is nearby there plz contact.

 

Plz circulate the brouchere to all concerned.

 


 

FOR DASH INSPECTORATE

U.G.DAS
DIRECTOR
804,BLUE DIAMOND COMPLEX,
NEAR FATEHGUNJ PETROL PUMP
FATEHGUNJ-BARODA GUJARAT-INDIA-02
9327201999,0265 2700454,
MOBILE 09825164743


--- On Sun, 20/4/08, Jignesh Patel <nacemail@gmail.com> wrote:
From: Jignesh Patel <nacemail@gmail.com>
Subject: [MW:723] AET type exchanger test ring
To: materials-welding@googlegroups.com
Date: Sunday, 20 April, 2008, 9:16 PM

Dear Friends,

 

I have seen few heat exchangers on this forum. I am an end user of heat exchangers in refinery. My query is related to test rings of exchangers.

 

One of our new units has AET type exchangers [pull through type]. These exchangers have a floating tubesheet [FTS] with bolt holes and the floating head cover [FHC] is directly bolted to the floating tubesheet. The problem with this is that we can't carry out shell test using a conventional test ring due to several bolt holes on the floating tubesheet. Conventional AES exchangers have backing rings pressing the FHC against the FTS.

 

I checked TEMA website and it says, test rings for such exchangers are possible and the bolt holes in the tubesheet need to be temporarily plugged. It also says refer to 4.13 (3) of TEMA. Unfortunately we don't have the latest edition of TEMA.

 

Does any one have experience with test rings [for shell test] for AET type exchangers? I would appreciate a generic drawing / scheme showing how to carry  out shell test of such exchangers.

 

Thanks in advance.

 

Thanks and regards,

 

Jignesh

Kuwait

 

For your virus protection, any attachments should be considered uncontrolled unless they are identified in the text. The sender does not accept liability for any virus introduced by this email or any attachment.

 



Best Jokes, Best Friends, Best Food. Get all this and more on Best of Yahoo! Groups. --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...