Can you please provide sketch of exchanger and design condition for the exchanger you have mentioned in your below mail.
Bellow is failing under shell side hydrotest pressure or tubeside hydrotest pressure?
Best regards,
Sunil S. Agrawal
Engineering & Design Tecnimont ICB
From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Prabhakar h
Sent: Sunday, April 06, 2008 12:09 PM
To: materials-welding@googlegroups.com
Subject: [MW:703] Should Thin Wall bellows to be tested...?
Hi everybody...
I have some problem in my design...
I was doing a Mechanical Dseign for a AES (TEMA type, single pass Heat Exchanger), where im supposed to design a Thin Wall Bellow on its Tube side.
The Design was carried out for the Design pressure and it was satisfactory...
The Problem is.. i was askeed by the client to producee calculations for Hydro test condition and my design fails in that condition.. My question is DO I HAVE TO CONSIDER THE TEST PR During my design?
anyone please clarify...
Prabhakar.H
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Sunday, April 20, 2008
[MW:722] Re: 703] Should Thin Wall bellows to be tested...?
hi Mr.Agarwal...
Sorry for replying late, as i was held up with my routines...
the bellow is failing @ shell side hydro test pressure.. which will be the external pr. of bellow..
i ve enclosed the sketch for better understanding...
please have a look and advice.
Prabhakar.H
On 4/11/08, Agrawal Sunil (Mumbai -Stequ) <S.Agrawal@ticb.com> wrote:
Subscribe to:
Post Comments (Atom)
[MW:35692]
Dear all Can I do MPI above painting surface for cs tank Regards, Sriram Srinivasan -- https://materials-welding.blog...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment