Dear Mr. Philip,
 
The 6GR position applicable for pipe welding and as know that pipe welding means done only from one side with out backing.  So the welder is qualified  without backing.  So he is qualified to weld any position  and butt joints with / without backing.  Your inerpreation is not correct.
 
N.V. PRASAD
WELDING ENGINEER
VELOSI CERTIFICATION
QATAR.

On Fri, Jul 2, 2010 at 3:59 PM, Philip, Taiye (Lagos) <Taiye.Philip@deltaafrik.com> wrote:

Hello gents,

 

 I have a query on butt joint welding with 6GR qualified welder. As per AWS D1.1 (2006) Table 4.10 Note d, 6GR qualified welder is qualified for all position. However, they are not qualified to weld production weld butt joint welded from one side without backing or welded from both side without backing. In this case, it is considered as single side welding without backing. Pls could some one in the house clarify more on these if I am right or wrong as per D1.1 interpretations?

 

 

Regards

Philip Taiye

Principal QA/QC Welding Engineer

(MIPs Quality Control)

DeltaAfrik Engineering Limited

2nd Floor, City Express Bank Building

Plot 1637 Adetokunbo Ademola Street

Victoria Island, Lagos  Nigeria

Phone: +234-1-461-8508, +2341-461-6137 ext. 1257
Cell: +234-(0)-803-803-1396
Fax: +234-1-262-2418

e-mail: taiye.philip@worleyparsons.com

 

 


*** WORLEYPARSONS GROUP NOTICE *** "This email is confidential. If you are not the intended recipient, you must not disclose or use the information contained in it. If you have received this email in error, please notify us immediately by return email and delete the email and any attachments. Any personal views or opinions expressed by the writer may not necessarily reflect the views or opinions of any company in the WorleyParsons Group of Companies."

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

No comments:

[MW:34916] Applicability of Impact requirement as per ASME B31.3

Dear All, Design code – ASME B31.3, Welding Code- ASME BPVC SEC IX Material  to be used used during Fabrication - SA 333Gr6 (P No.1 G...