RE: [MW:32571] Flushing & Cleaning Pressure for piping (Applicable code ASME B31.3 )

Dear Zafar,  Here my recommendations: Define the schedule of the pipe, define the length of the span for the flushing, and define the test time. Secure the pipe anchors and supports. Check that it does not generate induced vibration towards static equipment nozzles, as it can generate cracking of the weld. And most of all, be cautious. Regards,  Ramon Briceno  www.linkedin.com/in/ramonbriceno-metalengineer De: materials-welding@googlegroups.com <materials-welding@googlegroups.com> en nombre de Chaudhary Zafar Iqbal <chzaiqbal88@gmail.com> Enviado: jueves, 21 de octubre de 2021 4:30 a. m. Para: materials-welding@googlegroups.com <materials-welding@googlegroups.com> Asunto: [MW:32570] Flushing & Cleaning Pressure for piping (Applicable code ASME B31.3 )   Respected Experts , Good Day ! Design Pressure :3.5 Bar & Test Pressure as per isometric dw...

[MW:32570] Flushing & Cleaning Pressure for piping (Applicable code ASME B31.3 )

Respected Experts , Good Day ! Design Pressure :3.5 Bar & Test Pressure as per isometric dwgs : 5.5 Bar  Test Medium:Water  operating condition : Pressure : 0.4 Bar  Temperature : AMB  Pipe Size & material  : 6'' A 53 Gr B Seamless  My Question : is there any restriction in code to limits the test pressure during flushing with water as  our test pressure will be 7 BAR for flushing and also we need to report the same readings in report . PIPING SYSTEM – FLUSHING AND TESTING Report No.:   Item Description of Check Sub Contr. Contractor Company Sign Date Sign Date Sign Date 01 Limits of test in accordance with the scope listed on the attached test index and marked-up P&ID's   ...

Re: [MW:32568] API 650

As an additional note, I am referring to submerged arc welding for horizontal seams and wonder if there is a limit on the shell plate thickness which requires 2-side welding.  Patrick On Wed, 20 Oct 2021 at 11:25, Ying Piu Ng < ngyingpiu@gmail.com > wrote: Dear Experts, I am working on the construction of aboveground circular steel water storage tank. The thickness of the shell plate measures 25mm.  I wonder if there is any limit on the shell plate thickness which requires 2 side welding. Look forward to your kind advice. Regards Patrick On Sun, 28 Mar 2021 at 20:33, Pankaj Kolhe < pankaj.kolhe15@gmail.com > wrote: Yes On Fri, Jan 22, 2021 at 2:17 PM chitko khaing < chitkokhaing2009@gmail.com > wrote: Dear all  I am chit ko from Myanmar. i want to know " API 650 RT acceptance Criteria" refer to ASME VIII Division 1? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are ...

Re: [MW:32567] API 650

Dear Experts, I am working on the construction of aboveground circular steel water storage tank. The thickness of the shell plate measures 25mm.  I wonder if there is any limit on the shell plate thickness which requires 2 side welding. Look forward to your kind advice. Regards Patrick On Sun, 28 Mar 2021 at 20:33, Pankaj Kolhe < pankaj.kolhe15@gmail.com > wrote: Yes On Fri, Jan 22, 2021 at 2:17 PM chitko khaing < chitkokhaing2009@gmail.com > wrote: Dear all  I am chit ko from Myanmar. i want to know " API 650 RT acceptance Criteria" refer to ASME VIII Division 1? -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://gro...

Re: [MW:32561] ASME B31.3 process piping Hydro in Lieu of RT

Hi,  There's one option in B31.3,- U341.4.1. A weld coupon examination in accordance with para. U344.8 May be used in lieu of 5% random radiography/ultrasonic examination required in para. 341.4.1(b)(1) when the following  are employed in fabrication. 1. Autogenous automatic welding  2. Automatic orbital welding with the use of consumable insert rings. There is no option for hydrostatic in lieu of RT. Karthik Sent from Yahoo Mail for iPhone On Friday, October 15, 2021, 1:13 PM, Karthik <karthik6684@yahoo.com> wrote: Hi,  There's one option in B31.3,- U241.4.1. A weld coupon examination in accordance with para. U344.8 May be used in lieu of 5% random radiography/ultrasonic examination required in para. 341.4.1(b)(1) when the following  are employed in fabrication. 1. Autogenous automatic welding  2. Automatic orbital welding with the use of consumable insert rings. There is no option for hydrostatic in lieu of RT. Karthik Sent from Yahoo Mail for iPh...

Re: [MW:32561] ASME B31.3 process piping Hydro in Lieu of RT

tie in must to be radiofraphie or other NDE and its not include in hydro test  As per Para 345.2.3 (c) of ASME B31.3 you can either do  100% RT or 100% UT. If Project Specification asks for, you may have to  On Thu, 14 Oct 2021 at 14:25 Chaudhary Zafar Iqbal < chzaiqbal88@gmail.com > wrote: Dear Experts , due to time concentrate we are unable to do the RT as we need to arrange the RT crew and ID's process for site access  ........... as per drawing 5% RT is required . we can perform hydro of tie in joints ?  can you please advise for the reference from ASME B31.3  ?  Best Regards, Zafar Iqbal  00966544639978  -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discu...

[MW:32560] ASME B31.3 process piping Hydro in Lieu of RT

Dear Experts , due to time concentrate we are unable to do the RT as we need to arrange the RT crew and ID's process for site access  ........... as per drawing 5% RT is required . we can perform hydro of tie in joints ?  can you please advise for the reference from ASME B31.3  ?  Best Regards, Zafar Iqbal  00966544639978  -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAP9k9XcM6-QrnGrGm5%3DBN46HRJx_k6DKiaPBs6Pbpjw033JPSA%40mail.gmail.com .