Re: [MW:35690] Qualification of Unlisted materials using AWS D 1.1 - 2020Ed - reg

Pl qualify the combination in line with Drawing .


On Sat, 21 Jun 2025 at 12:10 PM, nagendran natarajan <nagend3484@gmail.com> wrote:
Dear all , 

I have a situation to Qualify single Bevel CJP - API 5L X 65 pipe with Plate API 2W Gr.50 PL1 , using structural Welding code AWS D 1.1. 
The Problem is API 5L X 65 is unlisted in AWS D 1.1 and API 2W is listed in Group 3.
AWS D1.1 says , PQR using any unlisted materials shall qualify for that particular combination only.
which means i have to go for pipe and plate combination for PQR. Curious to know whther anyone have done PQR for this situation?, If so pls throw some light..




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/3bd3cf09-a8d0-4d38-92f3-7d678aedd3adn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADder3PvicaODAmyvA3%2BfkBFveV%2BsuWAE%2BWR6b0QQH2nNhiVZw%40mail.gmail.com.

No comments:

[MW:35738] ASME IX WPS Qualification Query: GTAW + FCAW with Multiple PQRs

Dear Welding Experts, I'm currently preparing a Welding Procedure Specification (WPS) and have encountered a request to qualify a GTAW +...