Re: [MW:35673] Selection of Filler/Electrode.

i think that NICr3 is Inconel 600.
Inconel & Incoloy have vast differences in % Fe. content.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Sat, Jun 7, 2025 at 2:43 PM sridhar cn <sridharcn305@gmail.com> wrote:
For best results, use AWS A 5.14 ER Ni Cr-3 (Incoloy 800) filler wire for the weld metal when joining the Incoloy 800 tube to Super Duplex 
F53 SDSS tube sheet. This filler wire provides good compatibility with both materials, accommodates differences in thermal stability, and 
maintains corrosion resistance and mechanical strength. 
Alternatively, AWS A 5.14 ERNiCrMo-3 (Inconel 625) could be used for a Chloride rich or acidic atmosphere.
rgds,
C Sridhar.
------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------------

On Sat, 7 Jun 2025 at 09:28, HerculanJohn <hjpr820@gmail.com> wrote:
Dear Gentlemen,
Kindly advise me as we have tube to tubesheet joint.
Tube moc is incoloy 800
And tubesheet moc is F53 SDSS (Super duplex stainless steel).

For incoloy-800 -- P NO : 45
For F53 SDSS-- P NO: 10H

Which filler wire is applicable please suggest.

Best Regards,
John 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2B0nk_fb51cdvBvOdnrie0fFUtwwJEQoA0O%2BcAOjEm3s1wawoA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHo%3DYihM__UkyuXuD2TEAXnhkYY%2BEwz-kcoN%3DHdK%2B2PUkXh7Dg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMg6sQ4aU44AfYd0ykO%3DVZejK%3DP3TTdiavR%3D%3DOdPwuomw%40mail.gmail.com.

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...