Re: [MW:35644] Clarification Required on Welder Qualification – P-No. 8 vs. P-No. 45 (ASME Section IX)

New qualification is required 
Sent from my iPhone

On 29 May 2025, at 11:47 AM, Karuppa Samy <samyqc08@gmail.com> wrote:


Hello Everyone,

I would like to clarify whether a welder who is qualified using the GTAW process on P-No. 8 material is also permitted to weld P-No. 45 material, or if a separate qualification is required for P-No. 45.

Additionally, I would appreciate it if someone could provide a brief explanation regarding the relevant table in ASME Section IX that addresses this qualification range.

Your expert input on this matter would be highly appreciated.



<image.png>


Regards,
K. Karuppasamy


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJg1SznAZ74w2eF6jFi5ZU%2Bmmu%3DYq5v35c86CyCWB%3Dy6HZ7RKQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...