Re: [MW:35642] IP Joint

Many thanks Dhana. 

I am new to Aramco project. I will go through the specs. 

Regards 
Saurabh


On Mon, 26 May 2025 at 9:28 PM, Dhanabal Jalachandran <dhanabal.jalachandrann@gmail.com> wrote:
Greetings,

In Saudi Aramco projects, the term "IP" refers to the Initial Production weld for piping joints. As per the requirements of SAEP-324 (Welder Performance Qualification Procedure), every welder must perform a minimum of three (3) Initial Production (IP) welds following the successful completion of their Welder Qualification Test (WQT).

This process ensures that welders not only meet qualification standards in a controlled test environment but also demonstrate their proficiency in actual site conditions before being released for production welding activities.  

Reference - SAEP-324

Best Regards
Dhana

On Mon, May 26, 2025 at 7:27 PM Ganga Prasad <gangaprasad9010@gmail.com> wrote:
Greetings,

I think 'IP' joint means 'incomplete penetration'(partial penetration) joint.




On Mon, May 26, 2025, 7:30 AM 'Eugene Matsko' via Materials & Welding <materials-welding@googlegroups.com> wrote:
In essence, an IP pipe joint is any connection made between pipes that are sized using the IPS or NPS standards, regardless of the specific connection method.

Sent from my iPhone

On May 24, 2025, at 9:48 PM, Saurabh Jain <ensaurabh@gmail.com> wrote:


Hello experts,

I would like to know what is IP joints in piping(31.3)? 

Regards
Saurabh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADr-LL_mAcbc5GDt1TSd_Oip4ns3sqL_mS_AOtP4PyW7a9V9OQ%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/7BC10B8B-F349-4C33-B40E-20F56C6FB24A%40yahoo.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CACoqHbO4S8M1DgQCKJAatH4y40G4HY03Ryiwvr6BGxwEBKi8_Q%40mail.gmail.com.



--
Regards
Dhanabal Jalachandran

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAPLwtDcC-Li20S1EVK8pZ0AwUmt0WwLdhAr_aSu4bgeNjKLasA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CADr-LL9q%2BeJmd3NCTO-BcaK2bOvNFUTbK3JVdNcya3QbZfmSHQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...