Saturday, June 21, 2025

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen,
Kindly advise me as we have tube to tubesheet joint.
Tube moc is incoloy 800
And tubesheet moc is F53 SDSS (Super duplex stainless steel).

For incoloy-800 -- P NO : 45
For F53 SDSS-- P NO: 10H

Which filler wire is applicable please suggest.