We have a PQR qualified for P No.1, Gr.1 to 2, 45mm thk, PWHTd and Impact tested at -66 Deg C, where the holding temperature is 625 ± 25 Deg C, holding time is 450 Minutes.

It was an old PQR and I do not know the reason for such a long holding time kept during that time , as I am new to this company.

We have used this PQR for the fabrication of  a vessel, P No.1 Gr.1 & 2, design code is ASME Sec VIII Div-1, PWHT exists and Impact test is -29 Deg C.

But during heat treatment, the holding temperature is 640 Deg C, but the holding time is 750 Minutes, done by the PWHT subcontractor, even though we informed to keep holding time as 450 minutes with reference to the PQR.

As per ASME Sec IX, QW-407.4, especially this 750 minutes holding time still acceptable ?

We need to justify the client, if they ask to clarify.

Please advice.

Regards,
Saravanan Sornam,
S.Korea.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALV1rk%2ByLkQSxinhGz%3D8FE7WKLaXe2kLnfQiAWiqDfhgWT%2B2-A%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...