Re: [MW:35621] As a QC Level 1, I'm wondering if I'm qualified to:

Please check Standard ANSI / ASME N45.2.6 Qualifications of Inspection, Examination, and Testing Personnel for Nuclear Power Plants

 

René Alvarado


El vie, 16 may 2025 a la(s) 6:57 a.m., Desmond Meyer (meyerdesmond87@gmail.com) escribió:

Dear Experts,

I hope this email finds you well. I'm reaching out for advice on a current project where we're performing flux core welding. We need to qualify our welders and ensure compliance with relevant standards.

As a QC Level 1, I'm wondering if I'm qualified to:

1. Evaluate and qualify welders?
2. Write Procedure Qualification Records (PQR)?
3. Develop Welding Procedure Specifications (WPS)?
4. Conduct Welder Qualification Tests (WQT)?

Specifically, we're working with flux core welding, and I'd appreciate guidance on the requirements and best practices for welder qualification and documentation.

Could you please provide advice or point me in the direction of relevant resources?

Thank you for your expertise and assistance.

Best regards,

DESMOND 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKM3ENkVYsu3ge4sr_WQQC1RU_8%3DN6%2B54eUU1umt_p%3DJvQWnoA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHbC_j1VcaS3R4gRJDUJaC3whjq3Kf0H3CS1UH_v8LozWC3dqg%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...