Re: [MW:35610] DISSIMILAR WELDING IN STRUCTURAL

Yes, the WPS is okay for CS to SS fillet welding (P1 to P8) using ER309L, preferably by GTAW only since the thickness is less.

BR 
Deerendra 

On Wed, 14 May, 2025, 13:29 Akhilesh Kumar, <akhileshlikes@gmail.com> wrote:
Greetings Experts,
I would like to bring your attention to and clarification about the below-mentioned materials required for welding in the structural platform for Instrument support. In which required earthing clit/plate (6mm THK X 50mm H X 65mm W SS316)  to be welded with pipe (API 5L Gr B Thk- 5.54 MM) and channel (PFC 100x50x10mm THK). ASTM A 572 GR 50).
Could you please confirm that the mentioned piping WPS can be used for above mentioned ?

Thank you for your response and suggestion.
WBR,
Akhilesh K.
+918172813538

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAE1xz0NaaoTUsRBSx%3D7KYtG%2BDCmyr-S2gS2GwRomtpfzzWWjhg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAG0nF9E%2Boe9%3DrvkXGJGdUuN6trez6Wdve-0rgA6Bd9S%3D-ZUYKQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...