[MW:35583] 13% Cr L80 Type Drill Casing Pipe WPS/PWPS

Dear Experts 

i need to establish a WPS for 13% Cr L80 Drill Casing pipe with Er10 Electrode, client don't want PWHT can any one help me with PWPS or WPS if available 

Ravi Kumar 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/0b157a42-5eae-4e16-871e-8434b271c34bn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...