E-6010 / ER70S2
On Fri, May 2, 2025 at 3:01 PM Muthu ram N <muthuram25@gmail.com> wrote:
6010 and 7010Best Regards
Muthuram. N
Mechanical Engineer--On Fri, 2 May 2025 at 8:32 AM, Shivasankar A <shivasankar2593@gmail.com> wrote:Dear Friends,Can you suggest me the Welding consumable ( Both Filler Wire & Electrode) for Below materials,1. API 5L Gr. B + API 5L Gr. B =2. API 5L Gr X52 + API 5L Gr X52 =3. API 5L Gr X70 + API 5L Gr X70 =If any body having the WPS & PQR in the above materials. kindly share me for reference. These are the new materials for me. So Kindly help me guys.Regards,A.Shivasankar--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/46eccafa-c650-4998-96cc-0f33f512690fn%40googlegroups.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKdzwOqFraMStbygfi42SaAA4mSztU%3DEeFLEOFfWZ110tTMEOg%40mail.gmail.com.
Regards,
Chandrakant
B.E Mech.
ASNT Level II RT/UT/PT/MPT/CSWIP
GST -27AMOPP5962A1ZS
Patni Engineers. Mumbai. India
Patni Engineers. Mumbai. India
PED/2014/68/EU
welding shop AD2000/DIN EN ISO 3834
IBR Approved
Factory Addreess- Pl Call
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKLNAG7Ca38iqHFJyOKtDDHOSmD54CGRpsxk7jHtLWGXnkwPeg%40mail.gmail.com.
Comments