I have seen thus issue the slag impression after removal also due to improper rod heating and placing material in oxidation condition.

On Sat, 26 Apr 2025, 18:37 Nambirajan Avudaiappan, <nambirajanavudaiappan@gmail.com> wrote:

Dear Experts,

We are currently conducting FCAW qualification on a 25mm thick SA-36 material plate. However, we are facing issues with slag inclusion during the process.

Despite performing thorough cleaning after every pass, slag inclusions are still observed.
We kindly request your advice and recommendations on how we can take effective control measures to eliminate this problem.

Your expert guidance would be highly appreciated.

Thank you and best regards,

Nambirajan A

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJuyB2Xo-oR1On%3D5v6oiUvEPu-%2BG%2Bbzo%2Bf1DMR_3PXWXiEacuA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAGr8UaaMfgNgkdBa6oqz2M1cUZd5qjUOXW4ibAvCmMkp%2BQnESw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...