we have qualified WPS( P No 8 GR 1 To P NO 8 GR 1). Filler metal Er 316l ( Fno:6)
In our current project UNS S31254 ( PNO 8 Gr No 4)
We useing a filler wire ER2594 (Fno 6 )
Can we use above wps for this project with filler metal ER2594 Please guide me
CODE ASME SEC IX