Dear Elavarasan Mech,

For SA-312 UNS S31254 (Super Austenitic Stainless Steel), ErNiCrMo-3 is often a better choice of filler wire compared to ER2594. While ASME Section IX does not provide straightforward rules for filler wire selection, it is essential to rely on manufacturer recommendations or consult welding consumable catalogs for guidance. Additionally, a summarized electrode selection table, reflecting current industrial practices, is available in API 582.


Regards,
Babar Ghauri
Sr. Welding Engineer


On Tue, Apr 29, 2025 at 5:57 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
pl check Ano for ur new welding consumable.

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015, ISO 3834, EN 15085, 
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Apr 23, 2025 at 4:58 PM Elavarasan Mech <elavarasan1861994@gmail.com> wrote:
Dear All 
 Please clarify below 

we have qualified WPS( P No 8 GR 1 To P NO 8 GR 1). Filler metal Er 316l ( Fno:6)
 
In our current project UNS S31254 ( PNO 8 Gr No 4)
We useing a filler wire ER2594 (Fno 6 )


Can we use above wps for this project with filler metal ER2594  Please guide me 
CODE ASME SEC IX 





regards 
ELAVARASAN

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ymviaYs8wTi0ZC2v_L9PsxT9%3DRsHdQNgCDbJJSZsjdyug%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOxxD8z6aDo6M%2B%2BDyHgvckQps0D293WRuVx%2BQTfBmF2Pw%40mail.gmail.com.


--



Regards,

Babar Ghauri

+923455767300


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CALMZ9%2BqrwLbbEacFbKZLCG-yxTYJDFibTdeWLcCgy6e6JqwDxA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...