Yes
Best Regards,
Eng. Hany Nabil
Senior QA / QC Welding Engineer
Email: eng.hanynabil20@gmail.com
Egypt Mobile: 002-01225622022
This message, including any attachments, may contain confidential and privileged information for the sole use of the intended recipient(s). Review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient, or authorised to receive information on behalf of the recipient, please contact the sender by reply email, and delete all copies of this message. While we have taken reasonable precautions to ensure that this message and any attachments are free from viruses, we cannot guarantee that they are virus free and accept no liability for any damage caused by this message or any attachments. Messages sent or received through our networks may be monitored to ensure compliance with the law, regulation and/or our policies.
On Thu, Apr 24, 2025 at 2:33 PM venkateswara reddy Desireddy <dvreddy82@gmail.com> wrote:
--Dear experts ,Can I write single WPS with two PQR .PQR are different process. onePQR SMAW & one PQR SAWRegardsD.V.Reddy
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEabyKmVceU4rJSYo5xdwsb_EO_eUJ3Jk3k9OU9RkoKGiACnPQ%40mail.gmail.com.
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAP1YJmRjVCdAfTZtLfbhfaDH3%2B6tOxaXV4vGOSoA_vAM_A5OWA%40mail.gmail.com.
Comments