pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of ferrite.
On Wednesday, April 23, 2025 at 2:28:22 PM UTC+3 Elavarasan Mech wrote:
Dear AllPlease clarify belowwe have qualified WPS( P No 8 GR 1 To P NO 8 GR 1). Filler metal Er 316l ( Fno:6)In our current project UNS S31254 ( PNO 8 Gr No 4)We useing a filler wire ER2594 (Fno 6 )Can we use above wps for this project with filler metal ER2594 Please guide meCODE ASME SEC IXregardsELAVARASAN