Skip to main content

Re: [MW:35595] Welding Consumable Selection for the API Materials

Greeting.
It's dependent what process you are willing to use. Mostly common consumable are .

Api5L gr-60 to down Api 5l Gr 52 :
1.
Manual  root - 70S2 and filling capping E7018

2 down hill process 6010 root and filling capping 7010.

Api5l gr70 - 70S2 Filler Wire and E8018 for filling capping.

mGmaw process 70S-6





Regards,

Muhammad Azeem Iqbal
Welding QC Supervisor
053110-8577/0554453626/0590071467



On Fri, 2 May 2025, 12:31 Muthu ram N, <muthuram25@gmail.com> wrote:
6010 and 7010 

Best Regards
Muthuram. N
Mechanical Engineer



On Fri, 2 May 2025 at 8:32 AM, Shivasankar A <shivasankar2593@gmail.com> wrote:
Dear Friends,

Can you suggest me the Welding consumable ( Both Filler Wire & Electrode) for Below materials,  

1. API 5L Gr. B + API 5L Gr. B =
2. API 5L Gr X52 + API 5L Gr X52 = 
3. API 5L Gr X70 + API 5L Gr X70 = 

If any body having the WPS & PQR in the above materials. kindly share me for reference. These are the new materials for me. So Kindly help me guys.

Regards,
A.Shivasankar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/46eccafa-c650-4998-96cc-0f33f512690fn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAKdzwOqFraMStbygfi42SaAA4mSztU%3DEeFLEOFfWZ110tTMEOg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAHqH7yAyQLGjgNSE_z-hVqQVt%2B%3DkGmSRXdQGazMytLNVOFYQVw%40mail.gmail.com.

Comments