Thursday, February 13, 2025

Re: [MW:35430] Welding Qualification for Shell with Rod full Penetration Welding

This joint groove com fillet, set in joint. 
WPS: you can use dissimilar material plate WPS. WPS thickness qualification range and main shell thickness should be in the limits.
In this joint rod diameter not considered due to setin joint.
For set on joints only consider rod diameter or nozzle diameter for welder qualification.

Regards
D.V.Reddy
9493404456

On Mon, 10 Feb 2025, 1:44 pm Shivasankar A, <shivasankar2593@gmail.com> wrote:

Capture.PNG
Dear Friends,

Can you suggest me for a welding qualification for the above joint detail.

Material : Shell - SA 516 Gr.70
Rod : Duplex
Welding process: GTAW + SMAW

In my point of view, Plate to plate (Dissimilar) normal butt welding WPS & PQR is enough.  

Why I have a doubt is, here there is Diameter for Rod. So is there any Special Welding qualification for including the Diameter.

Please provide me the full step of Welding Qualification for the above Joint detail.


Regards,
A.Shivasankar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/c21ac9de-5d5f-4b97-91fd-882f63069a4bn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEabyKncNdiQk7vrhgvND9f-TCz4ppVS04T-27WpTwWcMy%2BB_w%40mail.gmail.com.

No comments:

[MW:35692]