[MW:35426] B31.3 Paragraph 331.1.3 Definition of Thicknesses Governing PWHT

Dear Expert ,
kindly help me to explain what mean control thickness in below paragraph 
331.1.3 Definition of Thicknesses Governing PWHT
(a) The term control thickness as used in Tables
331.1.1-1 and 331.1.3-1 is the lesser of
(1) the thickness of the weld
(2) the thickness of the materials being joined at the
weld or the thickness of the pressure-containing material
if the weld is attaching a nonpressure-containing material
to a pressure-containing material.
(b) Thickness of the weld, which is a factor in determining
the control thickness, is defined as follows:
(1) groove welds (girth and longitudinal) — the
thicker of the two abutting ends after weld preparation,
including I.D. machining
(2) fillet welds — the throat thickness of the weld
(3) partial penetration welds — the depth of the
weld groove
(4) material repair welds — the depth of the cavity to
be repaired
(5) branch welds — the dimension existing in the
plane intersecting the longitudinal axes, calculated as indicated
for each detail using the thickness through the weld
for the details shown in Figures 328.5.4-2 and 328.5.4-4.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/36ccc3ce-7626-4918-a901-111b3668a24an%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...