Wednesday, December 18, 2024

Re: [MW:35349] Cast-iron welding

Pl contact consumable supplier He will guide you 
There are consumable available for Cast iron .
Pre heating and consumable are addressed data sheets 
Vishwas
IWE

Sent from my iPhone

On 18 Dec 2024, at 4:39 PM, elams.rajan@gmail.com wrote:


Any advice for cast iron welding

--