Hii,
Which standard cover interruption during pwht 

On Sun, Dec 22, 2024, 4:41 PM Shekh Sadik <sadekurrahman.msbpl@gmail.com> wrote:
Hello Experts,
Can anyone provide me some assistance regarding the subject.

Query:
what are the effect of nitric acid and Sulphate in stainless steel pipe (material SS304)

Details:
Sample contains 8.6 wt% of Sulphate. Total titratable acidity of the sample is 35.6 wt% as nitric acid.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/7c23c7b7-c51d-4c4d-8cb0-843c644ea155n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAFm2zHuZEy5eHhU4M33t_8y%2BXLBbQbmUWEorHxenoZvOpbAhWg%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...