[MW:35330] Corrosion Rate criteria for material UNS N06022 nickel alloy

Team,
This is regarding material UNS N06022.

The corrosion Test is carried out as per ASTM G28 Method A.
The test result is 37.762 mpy (0.9592 mm/year).

May I know which standard provides acceptance criteria (range) for corrosion rate?

Regards,
Vivek

--