Skip to main content

Re: [MW:35126] Interpass temp

Hi sir

From where did you get this information 

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

From iPhone xs


On Mon, 15 Jul 2024 at 11:20 AM, Prathab P <prapoovins@gmail.com> wrote:

Dear,

As per ASME the preheating and interpass temperature is 95°C to 120°C.


On Sun, 14 Jul 2024, 23:30 krishnan T, <krishrev@gmail.com> wrote:
Reply i got From AI is below 

The interpass temperature when welding ASTM A572 Gr 50 with electrode E11018M (ENiCrMo-3) depends on the specific welding procedure and project requirements. However, here are some general guidelines:

- The interpass temperature for welding ASTM A572 Gr 50 typically ranges from 150°F to 300°F (65°C to 150°C).
- For electrode E11018M, the recommended interpass temperature is usually between 200°F to 250°F (90°C to 120°C).
- It's essential to consult the welding procedure specification (WPS) and the electrode manufacturer's recommendations for specific interpass temperature limits.
- Maintaining the appropriate interpass temperature helps prevent weld defects, ensures proper weld penetration, and achieves the desired mechanical properties.

Remember to always consult the relevant welding codes, standards, and project specifications for the specific interpass temperature requirements.

On Sun, 14 Jul, 2024, 21:06 R S, <ravangaoker.r@gmail.com> wrote:
Dear, 

this is specific electrode, E11018M, the manufacturer's recommendations may vary. Typically, the manufacturer's instructions should be followed.

On Sun, 14 Jul 2024 at 4:11 PM, saleem manhappulath <saleemm9526@gmail.com> wrote:
Dear All

    we are used material ASTM A572 Gr 50 and Electrode E11018m for PQR ,
Maximum Interpass how much we can mention in the WPS

Thanks & Best Regards
Saleem manhappulath

Mob:+966533595849
WhatsApp:+919526445936

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3Omv0KmS7%2B%2B-369L1K%2BOp5OHXZuj-RkTJ_n0_B2GmosZNLw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABJVWh-Wo9L%3Dea-NrgD8BBCWjBb8AUXnQLR7pngpzCkHBbafZA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2Bh%3Dzr23u1Qyfs4pYk%2BMg9dotFWxtsEPDr43zJkLyupyU7n%2BOw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFyvt4WpCLJbuXxdCW_gx_uNuSAN572KjteoUE4hmT00wLg%3DKA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKH3Omvs0t9EGqRKjStriKs%2Bxbxb9c6DvKdy1arkcbz0E92K5g%40mail.gmail.com.

Comments

Bhavik said…
thanks for sharing with us share more infor for our more knowledge

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

The Schaeffler and Delong diagrams for predicting ferrite levels in austenitic stainless steel welds

Introduction Ferrite is important in avoiding hot cracking in during cooling from welding of austenitic stainless steels. 'Constitution diagrams' are used to predict ferrite levels from the composition by comparing the effects of austenite and ferrite stabilising elements. The Schaeffler and Delong diagrams are the original methods of predicting the phase balances in austenitic stainless steel welds. Nickel and chromium equivalents A 'nickel equivalent' is calculated for the austenite stabilising elements and a 'chromium equivalent' ferrite stabilising elements. These are used as the axes for the diagrams, which show the compositional equivalent areas where the phases austenite, ferrite, martensite (and mixtures of these) should be present. Although intended to show the phase balance of weld fillers, these diagrams can also be used to illustrate the phase balance of the 'parent' material. There are different diagrams for dif...