Re: [MW:35103] EXCEL SHEET : WELD CONSUMABLE QUANTITY CALCULATOR



Thanks& Regards,

(Karthik)
Karthikeyan.S
M: +66-892512282


On Wednesday, July 3, 2024 at 04:19:49 PM GMT+7, Bharathi Raja.E <bharathiraja06.e@gmail.com> wrote:


  Dear Sir,

Thanks for sharing the file.
It is password protected, do you have the password


On Wednesday, April 26, 2023 at 1:42:38 PM UTC+5:30 williams p wilson wrote:
Dear Sir,

Thanks for sharing the file.
It is password protected, do you have the password

Thank You & Regards
Williams P Wilson
QA/QC Engineer
Please consider the environment before printing this message


On Fri, Nov 2, 2018 at 12:28 PM 'Karthik' via Materials & Welding <material...@googlegroups.com> wrote:
Hi,
The attached file might be useful to you.

Thanks& Regards,

 

(Karthik)

Karthikeyan.S

QA/QC Manager
Agon Pacific Co.,Ltd.
M: +66-655-174-397, +66-892-512-282

E-mail : karthi...@yahoo.com



On Friday, November 2, 2018, 1:41:24 PM GMT+7, MITHLESH <qa....@jshl.in> wrote:


HI SIR,
In attached file, ID means inch dia? and another thing is deposition rate of SAW not given. is it not applicable for SAW? 

On Thursday, November 5, 2015 at 10:39:05 AM UTC+5:30, Karthik wrote:
 Hi, 
The attached file might be useful to you
Thanks& Regards,
 
(Karthik)
QA/QC Manager 
CMI-Thai Services Co.,Ltd. 
50/35 Sermsuwan Road,Tambol Maptaphut 
Amphur Muang Rayong,Rayong 21150
Thailand
www.cmi-services.com 
Tel : +66 38 691 390-2 ext.103 
Fax : +66 38 682 338 
Mobile: +66 892512282 
E-mail : karth...@cmi-services.com
               Karth...@yahoo.com



On Wednesday, November 4, 2015 4:56 PM, waqas suleman <waqas....@gmail.com> wrote:


Dear Members,

I am also waiting for the same below requested file.

Regards,

Waqas Suleman
Mob. 00966 59 359 0798

On Tue, Nov 3, 2015 at 10:21 AM, Vikas Bhandari <vikas.bh...@gmail.com> wrote:
Hi

Can anyone share a standard excel sheet  for pipe butt weld consumable quantity calculation?

Many thanks

Best regards

Vb
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@ googlegroups.com.
To post to this group, send email to material...@ googlegroups.com.
Visit this group at http://groups.google.com/ group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ CACpSjOn%3DhNb3z324Ci-% 3D94bUSjpD7oVQUJBeWVokThmCi0GL %2Bg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/ optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@ googlegroups.com.
To post to this group, send email to material...@ googlegroups.com.
Visit this group at http://groups.google.com/ group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/ msgid/materials-welding/ CAKhANKjVn2-NoB%3D9nRZP2Fm% 3D8LyJWNoXzyZrpR_RAgvNefHRAQ% 40mail.gmail.com.
For more options, visit https://groups.google.com/d/ optout.






--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787

---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/ee7f90fc-2e60-41db-8715-3331d61a37cdn%40googlegroups.com
.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...