Dear all,

In the context of welding procedure qualification outlined by API 1104, it's important to note that the qualification of a butt weld does not extend automatically to branch and fillet welds. Each type of weld necessitates its own distinct qualification procedure.

Best regards,


Le sam. 30 mar. 2024 à 07:54, thulaib arakkal <thulaibwelding@gmail.com> a écrit :
Dear All,

In welding procedure qualification as per API 1104, does Butt Weld qualification also qualifies branch and fillet welds?.

Regards,

Thulaib

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL2L2JMkVLyYtdx0p-Pyuni4xchxmqY9QKjBT1D-syjF23V4mg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CANRRH0LF85RHAJogK-y4o49T5DvFp_XUF9YTiyUAMspr5nc4kQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...