[MW:34820] RE: 34813] Clarification in Rate of heating and cooling.

Hello,

 

Please see the response below.

 

Regards.

 

P. Goswami, P. Eng, IWE.

 

From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> On Behalf Of Gopalakrishnan G
Sent: Friday, March 15, 2024 2:39 AM
To: materials-welding@googlegroups.com
Subject: [MW:34813] Clarification in Rate of heating and cooling.

 

dear expert

I have to do WPS and PQR details given below

 

Test coupon

Thickness -50 mm

Material - IS 2062 E 350 C 

Code - ASME 

Position - 3G

Process - SMAW 

Electrode - E-7018

Impact = -20C @ 27J

Stress Relieving - 605+/- 10c

Rate of heating/cooling- 100c/hr.

 

Whether if Rate of heating / cooling is 100c/hrs will it affect the test result both UTS and Impact properties? : No, It's the Exposure time at the PWHT Temperature which matters most towards the UTS & Charpy Impact values. As a matter of fact, there is no need to maintain a cooling rate of 1000C/hr. You may increase the cooling rate to 150Deg C /hr or more.

 

As per UCS 56 ASME SEC 8 div 1 Max rate of heating and cooling 222c/hrs divided by max.metal thickness.

 

As my client need Rate of heating and cooling 100c/hrs.

 

Plz kindly clarify.

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOp_kKjwT0i_sWcf03H7PGvTrz0nXEFEmAmLKTsnX1y6Wwgzjg%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...