Re: [MW:34832] Inquiry about Single Bevel with Back Grinding

Dear Uday,

As per your question that one is called with backing only,Simple both side you are welding it is backing with strip or without strip plate it is called Backing .
Only one side welding without using any strip and welding is penetrated with other side it is called Without backing.

Regards,
S.MANIKANDAN  
08319656177
08718804461

 
  



On Mon, Mar 25, 2024 at 12:25 PM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
Double side welding is with Backing only. If u donot grind root & weld, it is without backing

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Sun, Mar 24, 2024 at 11:07 AM Chandra <chandrasekhar.palapala@gmail.com> wrote:
If you are doing back grinding or back gouging and grinding. It is considered as backing

Best Regards,
Chandra

On 23 Mar 2024, at 21.17, masna uday <masnauday4@gmail.com> wrote:


 Dear all , 

I am writing to seek clarification regarding the classification of single bevel with back grinding in terms of whether it is considered as with backing or without backing.

 Could you please provide information or guidance on this matter? Any insights or references you can share would be greatly appreciated. 

 Thank you for your attention to this inquiry. I look forward to hearing from you soon.


 Best regards, 

   


Masna Uday Kumar

masnaudayk4@gmail.com

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOOs2YZu42Lu509ky9oEa9rqxOV6o1SdX6E4eHLWyV8ha3Xc1A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/97B7C1C5-034E-4A61-B01E-936350D2F31B%40gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOXadkANnyOA_cn%3DArpBpafAc7wmk9YFs72aetY6jrWgg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL23xfsj2vgyri159YmftfFsWV-YHH--ZUeQGS8daSc9eaHqmw%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...