Re: [MW:34822] ASME P number for EEMUA 144


No, shall be assigned as UNLISTED material EEMUA 144 UNSC7060X 90/10 CuNi. which is not assigned in ASME Sec IX. 
Therefore the subject welding procedure cannot be qualified for material P34 as per Sec IX clause 403.11, which is an essential variable.

On Sun, 17 Mar 2024 at 10:48, thulaib arakkal <thulaibwelding@gmail.com> wrote:
Dear All,

Can we assign P number 34 to EEMUA 144 UNSC7060X 90/10 CuNi.

Regards,

Thulaib

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAL2L2JPwAzTU2hUC49U59gO7%2BqkMtNEv75S8LadfwyAcr94AVQ%40mail.gmail.com.


--
Best Regards,
Riju pathrose
QA/QC Engineer
Mob: +966534148879

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAq76B%3Do6G8hDcKerwTN7D9xeu5zwRNUFF82MUt%3DZ9rX08goSQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...