Re: [MW:34817] Clarification in Rate of heating and cooling.

For your question Whether if Rate of heating / cooling is 100c/hrs will it affect the test result both UTS and Impact properties?


Please control the heat input and string bead only. 


On Fri, Mar 15, 2024, 12:12 Gopalakrishnan G <gopal2408@gmail.com> wrote:
dear expert
I have to do WPS and PQR details given below

Test coupon
Thickness -50 mm
Material - IS 2062 E 350 C 
Code - ASME 
Position - 3G
Process - SMAW 
Electrode - E-7018
Impact = -20C @ 27J
Stress Relieving - 605+/- 10c
Rate of heating/cooling- 100c/hr

Whether if Rate of heating / cooling is 100c/hrs will it affect the test result both UTS and Impact properties?

As per UCS 56 ASME SEC 8 div 1 Max rate of heating and cooling 222c/hrs divided by max.metal thickness.

As my client need Rate of heating and cooling 100c/hrs.

Plz kindly clarify.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOp_kKjwT0i_sWcf03H7PGvTrz0nXEFEmAmLKTsnX1y6Wwgzjg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAGAT7zd4pJgyMiyA2i_spZ70fTRit1XjKBCV%2BG3wf20E9X%3DbNA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...