  1. 5 SFA-5.4 austenitic and duplex EXXX(X)-16 ... Why not this one. 

On Fri, Mar 15, 2024 at 9:25 AM Azmy Ashoush <marineweldingdpt@gmail.com> wrote:
Hi

F-No. For SFA A5.4 E2209-16 as per table QW-432 is 4

Thanks 


On Fri, Mar 15, 2024, 4:01 AM Prathab P <prapoovins@gmail.com> wrote:
Hi,

QW-432





On Thu, 14 Mar 2024, 13:02 Yutian Ren, <yutian.ren@gmail.com> wrote:
It can be E2209-16. 

P NAVEEN <pnaveen010@gmail.com> 于2024年3月13日周三 19:14写道:
Dear Sir's,

I am Planning to weld the SS2205 to SS 2205 material .   

Which filler rod ( SMAW ) we can use on that , If we can use the E 2209-16, What will be a F Number of that.

Thanks 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/8f61ea7b-e1bc-4b4a-b6f6-25601536267en%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMOy8oBBO3W96d-asFy-JRh-Bt%2BSdrKe5uhYJS-FLW%3DQXFKCdg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFyvt4VyWBz75f_TmrVNMgWhKnrfmWdzu%2BrNH02ceD%2BZpon23w%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B3QndGOkxX%2BM-nPuZcE1f-L0H6yNvLwP3%3DwbyFSrWg-7K0Gsw%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CABR6ro0pqGOB6Hm4q9Pt%2BOZ7zsVa_iG8SnqYCUXzNHKx0nBpuA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...