Re: [MW:34801] SS 310 TO SS 316 & SS316 TO SS304 Welding joint qualification & filler wire

Yes, Parminder singh & Kannayeram sir are right,sorry my mistake Filler: SS310 A no. is 9.

On Tue, Mar 5, 2024 at 11:21 AM Kannayeram Gnanapandithan <kgpandithan@gmail.com> wrote:
310 Ano is 9

On Tue, Mar 5, 2024, 8:07 AM Sahil musani <sahilmusani@gmail.com> wrote:
PQR Base metal SS304 (P8, Gr.1) TO SS304 (P8, Gr.1) & filler wire ER 308L (F No.6, A No.8)

ANS. 1) Yes you weld SS310  (P8, Gr.2) TO SS316  (P8, Gr.1) with the above PQR, Filler you have two options: ER310 or ER309.
ANS. 2) Yes you weld SS316  (P8, Gr.1) TO SS304  (P8, Gr.1) with the above PQR, Filler you have two options: ER308L or ER316L.

{Note: Your minimum design metal temperature shall not be colder than –155°F (–104°C)}

On Sat, Mar 2, 2024 at 2:57 PM Soumen Samanta <ssoumen05@gmail.com> wrote:
Dear Expert,

We have PQR base metal SS304 TO SS304 & filler wire ER 308L 
I have the following question 
1)Can we weld SS310 TO SS316 with the above pqr and what will be the filler for the same?
2)Can we weld SS316 TO SS304 with the above pqr and what will be the filler for the same?


Thanks in advance

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/33355d65-cf1b-48c3-bab5-3c223407725an%40googlegroups.com.


--
Regards,
Sahil Musani
(+91)-9033367145

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJZiFB94gYtiMNtQNrPtUJ3Z89v0oU5%2Bx%3DT8mA2gZdVr7PL5jA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePrEvDVR3zNzpzMBhfKZwNA5SjiGx0vct_R13Yw91%2BS%2Bw%40mail.gmail.com.


--
Regards,
Sahil Musani
(+91)-9033367145

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJZiFB9BOV%3DT9BZmYmQr2tRAL%2BXicxGP0KQc201VgLgFgNrOcA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...