Dear Gents,

I have to prepare a PQR as per below requirement:



Capture.JPG

Required your support for the selection of filler wire. The job is to cut header cap for inspection and weld it back for convection section.

As per my research we have selected ER-80S-B2 FOR ROOT AND CAPPING and E 8018-B2 for FILL UP and CAPPING.

--