[MW:34803] Re: ASME Sec IX interpretation record No # 17-3316

Record No # 17-3316 , This interpretation in not valid as on date.

On Wednesday 24 January 2024 at 19:16:19 UTC+5:30 vijay wrote:
Gents,

Fillet welding qualification according to ASME Sec IX 2023
PQR Material - EN 10025-2 S355JR to EN 10025-2 S275JR.

As per QW-424.1, the above materials are listed in the table QW/QB-422 and identified as below
EN 10025-2 S355JR - P-No.1, G.No.2
EN 10025-2 S275JR - P-No.1, G.No.1  

The proposed WPS shall cover one metal from the P-No.1 to any metal from the P-No.1 for the range of qualification.

However referring to ASME Sec IX interpretation record No # 17-3316 (attached), the interpretation seems different for Material SA/EN 10028-2 P355GH. 

Please clarify, if my understanding is correct.

Regards,
Vijay

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/9e951b64-55d1-47a9-bbbe-0c6dbf6f4cban%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...