Re: [MW:34673] Tube to Tubesheet weld- MLP value Inquiry

Dear sir,

MLP value shall be as per Design requirement or client specification/requirement.

Design concurrence required if client specification is silent for MLP Value.

On Sat, Dec 2, 2023 at 11:51 PM PARAI Reaction Channel <saravanshyla@gmail.com> wrote:
Dear Sirs,

We are fabricating a heat exchanger , designed as per ASME Sec VIII Div-1, 2021 Ed. 

with SS 304 Tube to Tubesheet welds, designed as per ASME Sec VIII Div-1, UW-20.1 "C " joint , strength weld type with 2 passes of GTAW welded from root.

We did PQR recently as per ASME Sec IX QW-193 2021 ED. requirements.

with ref. to the below joint sketch used for the actual weld joint , welded in the heat exchanger which is referred from the fabrication drawing,

for the PQR,  that is for MLP value as per ASME Sec IX QW-193.3 , can we use 0.7xt , where tube thk is 2.11 mm , so can we accept MLP as min. 1.48mm for all 10 tube welds?

Or from the root, the throat value shall be 4 x0.7, that is Min. 2.8mm for MLP based on the below sketch with leg size 2 mm and bevel depth 2 mm, totally 4mm weld ?

So which minimum value shall be used for acceptance , either 1.48 Or 2.8 mm for the MLP based on the above statements?

The actual measured MLP values received are 2.6 to 3.2 mm from the test lab, for 10 tube welds .



Please reply with your opinion for MLP value acceptance, before I submit these test report values to ASME AI for his review and stamp on the PQR.

Thanks and Regards,
Saravanan Sornam,
S.Korea.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CALV1rkJvn8pONjW8rCBd3rBJBO3KUXhgxt1WaF2iisH7nnLR1A%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADXbd_fYr-zxcm08SPoBAPykC8P%2Bxj6gYpjQdNi1gyRKeOh73w%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...