Re: [MW:34684] Impact testing - V NOTCH CHARPY. Recommendation

Normally either from the Process or Mechanical Designer will provide the MDMT ( Minimum Design Metal Temperature) - it is the lowest temperature attained by the Material either due to Process conditions / Environmental conditions / upset conditions. So Impact testing has to be performed at MDMT.

Charpy Impact values for Full size specimen (10x10x55) will be specified either by the Design Code  or superceded by the Client specification if provided. Test Temperature MDMT.

A Snap shot of ASME B 31.3 is given as example below.

Inline image

Thanks & Regards

J.Gerald Jayakumar



On Wednesday, 6 December, 2023 at 09:34:42 am IST, Prathamesh Patkar <prathameshpatkar@swastikindustriesindia.in> wrote:


Dear Sir,

Thank you for the response.

I had one more query. Are there any acceptance criteria for minus temperature? eg... the specimen should sustain 12 J impact at -20c in order to qualify. 



On Mon, Dec 4, 2023 at 5:30 PM 'james gerald' via Materials & Welding <materials-welding@googlegroups.com> wrote:
A Charpy Impact test is not required for specimen thickness less than 2.5mm.

Subsize specimens can be machined from the Pipe OD 60mm and thickness 5.5mm. Please check with the Mechanical testing lab.

Please refer to ASME Sec.IIA section SA-370.

If specimen thickness exceeds 80% during machining from the original size, temperature reduction according to the Applicable Code shall be applied.

For subsize specimens Impact values refer to snap shot.

Inline image


Thanks & Regards

J.Gerald Jayakumar




On Monday, 4 December, 2023 at 05:06:28 pm IST, Prats <prathameshpatkar@swastikindustriesindia.in> wrote:


Hello,

We have an impact testing requirement to be done on a pipe with an outer diameter of 60mm and a thickness of 5.5mm. 

What specimen size should we select for the testing? As the standard "ASTM E23-23A" states, specimen size should be 55L x 10W x 10 thick. We are a bit confused regarding the specimen size...has anyone faced a similar issue? please recommend 

Moreover, the specimen should sustain 27 J. 

Please help.

Thanks & Regards 
Prats

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d6ea2566-4818-419b-9dcf-d307c61bab53n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/598336985.6110574.1701690837182%40mail.yahoo.com.


--

Regards,




--
Thanks & Regards
Prathamesh S Patkar

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAC4daO1FWBtE5gfLNgNYqhsVg%2Bu0V475C3r53uDxgj82GDtq8A%40mail.gmail.com.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...