Intermediate buttering on P91 bevel to be done and complete the PWHT. 

Later on weld SS to inconel. 

PQR for guttering with PWHT is required. 

On Fri, 17 Mar 2023, 17:55 HerculanJohn, <hjpr820@gmail.com> wrote:
Dear Experts,
We are doing welding for Sa335 P91 to A182 F316 material. As per Wps Gtaw + smaw is welding sequence. 
Filler is ERNICR-3 And ENICrFe3. But Electrode we are using ENiCrFe2. 
During Gtaw welding there was no problem smooth welding but once me started Smaw than the electrode is not getting fused properly material is thrown out. 
We are maintaining proper interpass continously as per Wps. 
Kindly provide us valuable feedback.
Thanks & Regards,
John Rodrigues 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2B0nk_er6yvyhxEEYZD9J98prJhWpTvecvDRrzNFMCSh2vVA0g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEzKD3J1FasrcqiqaOqY%3DAuF0UJ2913XgXXATKdO_jFAM231MA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...