Re: [MW:34062] PQR for stainless steel with Duplex stainless steel

Sir.

1. What Group of SS and DSS?
2. Welding process? 
3. What method did you use for the Corrosion test?
4. Temperature: your client requirement for a test?
5. Heat input while welding, Interpass temperature?
6. What type of Argon is used for Purging Gas and shielding?
7. Branch of welding consumable. 
8. What type of chemical is used for pickling and passivation? 

Please reference API 582 for correctly chosen welding consumable as per your base metal and design as per project specification requirement. 

Vào Th 5, 9 thg 3, 2023 vào lúc 12:09 mohammed hashif pattambi <mohammedhashif786@gmail.com> đã viết:
Gents,

during PQR for WPS of SS to DSS using filler Er Ni Cr MO-10, Corrosion test is failing. can i get any advise and suggestion on this.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/099b14b7-c726-47f7-a62a-5466c81ff2acn%40googlegroups.com.


--
Best & Regard
Pham Thanh Tinh
QC Manager
China National Chemical Engineering Third Co.LTD
South Ghawar Gas Separation Plant & Associated Facilities Project
Mobile phone +966. 556802308 


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAEVAJwaCzo5Xts2nQyz8zsDezk0d1RoU0m%3Dtz-NxohmyvdX%2BiA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...