Re: [MW:34053] FILLER WIRE FOR SA516 GR.70 TO SB409UNSNO8810

Hi, the recommended filler metal for welding SA516 Gr.70 to SB409 UNS N08810 is a nickel-based alloy filler metal, such as Inconel 82 (AWS A5.14 ERNiCr-3) or Inconel 625 (AWS A5.14 ERNiCrMo-3). These filler metals are commonly used for welding dissimilar metals with high resistance to corrosion and high-temperature applications.

On Thu, Mar 2, 2023 at 8:36 AM sujit kumar <sujitkumar19942@gmail.com> wrote:
Dear all,

What filler wire we have to use to welding of SA516 GR.70 TO SB409UNSNO8810




Best Regards.
S.K

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFonYWMxEnVrD2tCb4CXihObGTnhBLX02cFe8L0KQNePCCezMA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAFhOWxYYOkzwVFxTpv08ToFnYN%2Ba5%3Di5KTakb3G%2BisGOLzyGyA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...