As per QW 404.37, A no is not essential /Not applicable for this Non ferrous  Filler metal. Only F no is essential, which is  F34  which comprise 90/10, 70/30 also as per SFA 5.7.
 So No New PQR is required. 

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Wed, Mar 1, 2023 at 3:29 PM Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:
This non ferrous weld metal.
What is the F number of PQR  filler metal?
If PQR filler metal's F number and Production joint filler metal's F number  is same ,then new PQR is not required 
Thanks
Vishwas -IWE 
On Friday, February 24, 2023 at 3:23:47 PM UTC+5:30 mohit aggarwal wrote:
Dear Experts,

We have equipment of weld overlay with 90/10 CuNi composition, but we have Procedure is only with 70/30 CuNi consumable.

As per QW-404.37 clause our AI asked to requalify the procedure due to change of consumable.

I have query can we do weld overlay of 90/10 with 70/30 consumable or we will have qualify new procedure for the same.


Regards,
Mohit Aggarwal
Welding Engineer

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/111d0d70-5570-42f9-8bfe-b914bf7c01b8n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4ePwq1vTGenRZ%2B3Wa0FqwL7Urk_oL-FvLAdraxXitzY2uQ%40mail.gmail.com.

No comments:

[MW:35754] interpration

  Interpretation #: BPV IX-18-34  Record Number: 18-771  Subject Description: SC IX; QW-401.1 and QW-403.6 - Thickness Range Qualified for I...