[MW:34104] SA266 GR4N 4 Cycle SPWHT

Hi 

Client has required 4 cycle for SA266 GR4N, They requested the certificate shall included all required test at both conditions, min and max simulated PWHT Cycles,
Our forging mill has issued MTC with mechanical property, before PWHT and after PWHT But they commented " test after SPWHT performed after 4 cycles(max condition-i think after 4 times we mentioned the result as after SPWHT) and missing test after min condition"(I think there is missing test result of min SPWHT condition)

Could anyone give us idea how to solve this issue and what test result shall be added 

Can we say min and max SPWHT? We performed 4 times of SPWHT as client's request.. 

what you guys think min SPWHT condition?

Regards,
ham

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/e0257065-b095-4a75-8729-26977b86f5a8n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...