[MW:34076] Re: SS304 HEAT TREATMENT PROCEDURE

Solution heat treatment follow quenching.
You also see in material spec ASTM A312 TP304.
Regarding rolling from plate with 10mm. it may not apply PWHT for this material type.

On Monday, March 20, 2023 at 9:59:22 AM UTC+7 Ganesh Rao wrote:
Dear Expert,

We looking for PWHT Procedure for material SS304.could any one can share the procedure urgently?
Pipe thickness : 10mm
Pipe OD : 1260mm
We need to do hot tapping on this pipe 


From,
Ganesh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/c0fff36b-67a6-48f8-bd11-01e01bf15ae8n%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...